The role of transverse speed on deposition height and material efficiency in laser deposited titanium alloy
- Mahamood, Rasheedat M., Akinlabi, Esther Titilayo, Shukla, Mukul, Pityana, Sisa
- Authors: Mahamood, Rasheedat M. , Akinlabi, Esther Titilayo , Shukla, Mukul , Pityana, Sisa
- Date: 2013
- Subjects: Additive manufacturing , Laser metal deposition , Material efficiency , Titanium alloy
- Type: Article
- Identifier: uj:4895 , http://hdl.handle.net/10210/12609
- Description: The most commonly used aerospace titanium alloy, Ti6Al4V, was deposited on Ti6Al4V plate of dimension 72 x 72 x5mm. The laser power of 3 kW, powder flow rate of 1.44 g/min and gas flow rate of 4 l/min were used throughout the deposition process. The transverse/ scanning speed was varied between 0.005 to 0.095 m/sec according to established result of the preliminary study that produces full dense and pore free deposits. The mass of the deposited powder was obtained by weight the substrate before deposition and reweighing after deposition. The substrate and the deposits were thoroughly cleaned using wire brush and acetone to remove unmelted powder particles from the surface of the substrate and the deposit. The height and width of the deposits were measured with Venier Caliper and the material efficiencies were determined using developed equations. The effect of the scanning speed on the material efficiency and deposit height were extensively studied and the results showed that for the set of processing parameter used in this study the optimum scanning speed is approximately 0.045 m/sec.
- Full Text:
- Authors: Mahamood, Rasheedat M. , Akinlabi, Esther Titilayo , Shukla, Mukul , Pityana, Sisa
- Date: 2013
- Subjects: Additive manufacturing , Laser metal deposition , Material efficiency , Titanium alloy
- Type: Article
- Identifier: uj:4895 , http://hdl.handle.net/10210/12609
- Description: The most commonly used aerospace titanium alloy, Ti6Al4V, was deposited on Ti6Al4V plate of dimension 72 x 72 x5mm. The laser power of 3 kW, powder flow rate of 1.44 g/min and gas flow rate of 4 l/min were used throughout the deposition process. The transverse/ scanning speed was varied between 0.005 to 0.095 m/sec according to established result of the preliminary study that produces full dense and pore free deposits. The mass of the deposited powder was obtained by weight the substrate before deposition and reweighing after deposition. The substrate and the deposits were thoroughly cleaned using wire brush and acetone to remove unmelted powder particles from the surface of the substrate and the deposit. The height and width of the deposits were measured with Venier Caliper and the material efficiencies were determined using developed equations. The effect of the scanning speed on the material efficiency and deposit height were extensively studied and the results showed that for the set of processing parameter used in this study the optimum scanning speed is approximately 0.045 m/sec.
- Full Text:
Characterizing the effect of processing parameters on the porosity of laser deposited titanium alloy powder
- Mahamood, Rasheedat M., Akinlabi, Esther Titilayo, Shukla, Mukul, Pityana, Sisa
- Authors: Mahamood, Rasheedat M. , Akinlabi, Esther Titilayo , Shukla, Mukul , Pityana, Sisa
- Date: 2014
- Subjects: Laser metal deposition , Medical implants , Porosity , Processing parameters , Titanium alloy
- Type: Article
- Identifier: uj:4739 , ISSN 2078-0966 , http://hdl.handle.net/10210/11725
- Description: Laser Metal Deposition (LMD) is an additive manufacturing technique that produces parts layer by layer directly from the Computer Aided Design (CAD) file. Highly customized parts with complex shapes such as medical implants can well be manufactured using the LMD process. LMD has been used to produce a wide range of patient specific (customized) parts. Porous parts are of particular importance as medical implants because they can potentially aid the healing process and proper integration of the implant with the body tissues. In this research porous samples of titanium alloy (Ti6Al4V) were produced using the LMD process. Spherical shaped Ti6Al4V powder of particle size ranging between 150 to 200 μm was used. The effect of laser power and scanning speed on the shape, size and degree of porosity of the deposited tracks was investigated. The results showed that as the laser power was increased and the scanning speed decreased, the degree of porosity was reduced. The size of the porosity was also found to reduce as the laser power was increased.
- Full Text:
- Authors: Mahamood, Rasheedat M. , Akinlabi, Esther Titilayo , Shukla, Mukul , Pityana, Sisa
- Date: 2014
- Subjects: Laser metal deposition , Medical implants , Porosity , Processing parameters , Titanium alloy
- Type: Article
- Identifier: uj:4739 , ISSN 2078-0966 , http://hdl.handle.net/10210/11725
- Description: Laser Metal Deposition (LMD) is an additive manufacturing technique that produces parts layer by layer directly from the Computer Aided Design (CAD) file. Highly customized parts with complex shapes such as medical implants can well be manufactured using the LMD process. LMD has been used to produce a wide range of patient specific (customized) parts. Porous parts are of particular importance as medical implants because they can potentially aid the healing process and proper integration of the implant with the body tissues. In this research porous samples of titanium alloy (Ti6Al4V) were produced using the LMD process. Spherical shaped Ti6Al4V powder of particle size ranging between 150 to 200 μm was used. The effect of laser power and scanning speed on the shape, size and degree of porosity of the deposited tracks was investigated. The results showed that as the laser power was increased and the scanning speed decreased, the degree of porosity was reduced. The size of the porosity was also found to reduce as the laser power was increased.
- Full Text:
- «
- ‹
- 1
- ›
- »